Forgings, Fasteners, Boltings, Stud Bolts, Screws, Nuts
ASTM A1099 specification covers modified high-strength alloy steel forgings and rolled and forged bar for oil and gas pressure vessels and oilfield equipment. See Appendix X1. Oil and gas product specifications for which this material is intended include, but are not limited to, the following:
API 6A Specification for Wellhead and Christmas Tree Equipment and Errata,
API RP 6AR Recommended Practice for Repair and Remanufacture of Wellhead and Christmas Tree Equipment,
API 16A Specification for Drill-Through Equipment,
API 16R Specification for Marine Drilling Riser Couplings,
API 17D Specification for Subsea Wellhead and Tree Equipment and Errata,
API 8C Specification for Drilling and Production Hoisting Equipment.
Supplementary requirements are provided for use when additional testing or inspection is desired. These shall apply only when specified individually by the purchaser in the order.
In the case of conflict between a requirement of this specification and a requirement of referenced general specifications, this specification takes precedence. In the case of conflict between a requirement of the product specification or a requirement of this specification and a more stringent requirement of the purchase order or contract, the purchase order or contract take precedence. The purchase order or contract requirements shall not take precedence if they, in any way, violate the requirements of the product specification or this specification, for example, by the waiving of a test requirement or by making a test requirement less stringent. In the case of conflict in terminology between API standards and Terminology A941, Terminology A941 definitions shall be applied.
Units—The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in nonconformance with the standard.
ASTM A1099 specification is expressed in both inch-pound units and in SI units; however, unless the purchase order or contract specifies the applicable M specification designation (SI units), the inch-pound units shall apply.
Grade | C | Mn | P | S | Si | Cr | Mo | Ni | Cu | V | Ti | Al | Sn | As | Sb | Pb | Bi | N | H | O | Nb (Cb) |
B |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
ASTM A1099 F22OF | 0.10- 0.15 |
0.30- 0.60 |
0.015 | 0.010 | 0.15- 0.50 |
2.0- 2.50 |
0.87- 1.13 |
0.50 | 0.25 | 0.04 | 0.025 | 0.055 | 0.015 | 0.020 | 0.020 | 0.010 | 0.010 | 0.0120 | 2 PPM |
25 PPM |
0.02 | 0.0005 |
ASTM A1099 F22OFA | 0.15- 0.20 |
0.40- 0.80 |
0.015 | 0.010 | 0.50 | 2.0- 2.50 |
0.90- 1.10 |
0.50 | 0.25 | 0.04 | 0.025 | 0.055 | 0.015 | 0.020 | 0.020 | 0.010 | 0.010 | 0.0120 | 2 PPM |
25 PPM |
0.01 | 0.0005 |
ASTM A1099 4130OF | 0.25- 0.33 |
0.60- 0.90 |
0.015 | 0.010 | 0.20- 0.35 |
1.20- 1.50 |
0.65- 0.75 |
0.25 | 0.25 | 0.04 | 0.025 | 0.055 | 0.015 | 0.020 | 0.020 | 0.010 | 0.010 | 0.0120 | 2 PPM |
25 PPM |
0.02- 0.05 |
0.0005 |
ASTM A1099 8630OF | 0.27- 0.33 |
0.80- 0.95 |
0.015 | 0.010 | 0.20- 0.35 |
0.85- 1.00 |
0.35- 0.45 |
0.80- 0.90 |
0.25 | 0.04 | 0.025 | 0.055 | 0.015 | 0.020 | 0.020 | 0.010 | 0.010 | 0.0120 | 2 PPM |
25 PPM |
0.02 | 0.0005 |
|
Grade | Class | Tensile (psi min) | [MPa minimum] | Yield (psi min % min at 0.2 % offset) | [MPa minimum] | Elongation (% min) | Reduction (% min) | Hardness (HBW) | Charpy V-Notch at 0°F [-20°C] (ft-lbf minimum average) | [J minimum average] | Charpy V-Notch (ft-lbf minimum single value) | [J minimum single value] |
---|---|---|---|---|---|---|---|---|---|---|---|---|
ASTM A1099 Grade F22OF | 75 | 95 000 | [650] | 75 000 | [525] | 18 % | 35 % | 197-237 | 31 ft-lbf | [42 J] | 24 ft-lbf | [32 J] |
80 | 100 000 | [700] | 80 000 | [550] | 18 % | 35 % | 207-237 | 31 ft-lbf | [42 J] | 24 ft-lbf | [32 J] | |
85 | 105 000 | [725] | 85 000 | [575] | 18 % | 35 % | 217-237 | 31 ft-lbf | [42 J] | 24 ft-lbf | [32 J] | |
ASTM A1099 Grade F22OFA | 105 | 125 000 | [850] | 105 000 | [725] | 18 % | 35 % | 269-302 | 31 ft-lbf | [42 J] | 24 ft-lbf | [32 J] |
ASTM A1099 Grade 4130OF | 60 | 85 000 | [575] | 60 000 | [425] | 20 % | 40 % | 174-237 | 31 ft-lbf | [42 J] | 24 ft-lbf | [32 J] |
75 | 95 000 | [650] | 75 000 | [525] | 18 % | 35 % | 197-237 | 31 ft-lbf | [42 J] | 24 ft-lbf | [32 J] | |
80 | 100 000 | [700] | 80 000 | [550] | 18 % | 35 % | 207-237 | 31 ft-lbf | [42 J] | 24 ft-lbf | [32 J] | |
95 | 105 000 | [725] | 95 000 | [650] | 17 % | 35 % | 217-255 | 30 ft-lbf | [41 J] | 22 ft-lbf | [30 J] | |
110 | 125 000 | [825] | 110 000 | [750] | 16 % | 35 % | 269-302 | 30 ft-lbf | [41 J] | 22 ft-lbf | [30 J] | |
125 | 135 000 | [925] | 125 000 | [850] | 15 % | 35 % | 277-321 | 30 ft-lbf | [41 J] | 22 ft-lbf | [30 J] | |
ASTM A1099 Grade 8630OF | 75 | 95 000 | [650] | 75 000 | [525] | 18 % | 35 % | 197-237 | 31 ft-lbf | [42 J] | 24 ft-lbf | [32 J] |
80 | 100 000 | [700] | 80 000 | [550] | 18 % | 35 % | 207-237 | 31 ft-lbf | [42 J] | 24 ft-lbf | [32 J] | |
85 | 105 000 | [725] | 85 000 | [575] | 18 % | 35 % | 217-237 | 31 ft-lbf | [42 J] | 24 ft-lbf | [32 J] | |
95 | 115 000 | [800] | 95 000 | [650] | 17 % | 35 % | 241-293 | 20 ft-lbf | [27 J] | 15 ft-lbf | [20 J] | |
100 | 120 000 | [825] | 100 000 | [700] | 16 % | 35 % | 248-302 | 20 ft-lbf | [27 J] | 15 ft-lbf | [20 J] | |
110 | 130 000 | [900] | 110 000 | [750] | 16 % | 35 % | 269-302 | 20 ft-lbf | [27 J] | 15 ft-lbf | [20 J] | |
120 | 145 000 | [1000] | 120 000 | [825] | 15 % | 30 % | 302-352 | 20 ft-lbf | [27 J] | 15 ft-lbf | [20 J] | |
135 | 150 000 | [1025] | 135 000 | [925] | 15 % | 30% | 321-375 | 20 ft-lbf | [27 J] | 15 ft-lbf | [20 J] |
Material | NormalizingA | AustenitizingA | Quench Media | Tempering MinimumB |
---|---|---|---|---|
F22OF Class 75 | 1675-1750°F [900-950°C] |
1650-1725°F [900-950°C] |
Water/polymer/oil | 1225°F [650°C] |
F22OF Class 80 | 1675-1750°F [900-950°C] |
1650-1725°F [900-950°C] |
Water/polymer/oil | 1200°F [650°C] |
F22OF Class 85 | 1675-1750°F [900-950°C] |
1650-1725°F [900-950°C] |
Water/polymer/oil | 1175°F [625°C] |
F22OFA Class 105 | 1675-1750°F [900-950°C] |
1650-1725°F [900-950°C] |
Water/polymer/oil | 1100°F [600°C] |
4130OF Class 60 | 1600-1700°F [875-925°C] |
1575-1650°F [850-900°C] |
Water/polymer/oil | 1250°F [675°C] |
4130OF Class 75 | 1600-1700°F [875-925°C] |
1575-1650°F [850-900°C] |
Water/polymer/oil | 1200°F [650°C] |
4130OF Class 80 | 1600-1700°F [875-925°C] |
1575-1650°F [850-900°C] |
Water/polymer/oil | 1200°F [650°C] |
4130OF Class 95 | 1600-1700°F [875-925°C] |
1575-1650°F [850-900°C] |
Water/polymer/oil | 1125°F [600°C] |
4130OF Class 110 | 1600-1700°F [875-925°C] |
1575-1650°F [850-900°C] |
Water/polymer/oil | 1075°F [575°C] |
4130OF Class 125 | 1600-1700°F [875-925°C] |
1575-1650°F [850-900°C] |
Water/polymer/oil | 1050°F [575°C] |
8630OF Class 75 | 1600-1700°F [875-925°C] |
1575-1650°F [850-900°C] |
Water/polymer/oil | 1225°F [650°C] |
8630OF Class 80 | 1600-1700°F [875-925°C] |
1575-1650°F [850-900°C] |
Water/polymer/oil | 1200°F [650°C] |
8630OF Class 85 | 1600-1700°F [875-925°C] |
1575-1650°F [850-900°C] |
Water/polymer/oil | 1200°F [650°C] |
8630OF Class 95 | 1600-1700°F [875-925°C] |
1575-1650°F [850-900°C] |
Water/polymer/oil | 1075°F [575°C] |
8630OF Class 100 | 1600-1700°F [875-925°C] |
1575-1650°F [850-900°C] |
Water/polymer/oil | 1075°F [575°C] |
8630OF Class 110 | 1600-1700°F [875-925°C] |
1575-1650°F [850-900°C] |
Water/polymer/oil | 1050°F [575°C] |
8630OF Class 120 | 1600-1700°F [875-925°C] |
1575-1650°F [850-900°C] |
Water/polymer/oil | 1050°F [575°C] |
8630OF Class 135 | 1600-1700°F [875-925°C] |
1575-1650°F [857.2-898.8°C] |
Water/polymer/oil | 1025°F [550°C] |
|
S3 | Surface NDE Examination |
---|---|
S4 | Macroetch |
S5 | Specimen Orientation |
S6 | Special Impact Requirements |